Harper International
Three graphite products systems (ultrahigh-temperature graphite rotary, graphite Harper HearthT and graphite pusher thermal system) facilitate spherical graphite production for batteries, pitch-based carbon fiber, metallic carbide powders and non-oxide ceramic sintering. The Harper Hearth operation has eight patented features that allow it to provide comprehensive time-at-temperature uniformity at minimal operating cost. The load carrier reduces load thermal mass, improves temperature uniformity and redistributes compressive stress and wear surfaces away from potentially corrosive or erosive environments.
Graphite Products
October 9, 2001
No Comments