Metals-India (www.metalsindia.com) added an Abar Ipsen TurboTreater that features acetylene vacuum carburizing technology. The furnace offers vacuum hardening, vacuum carburizing and vacuum carbonitriding.
Metals-India (
www.metalsindia.com) added an Abar Ipsen TurboTreater that features acetylene vacuum carburizing technology. The furnace offers vacuum hardening, vacuum carburizing and vacuum carbonitriding. The TurboTreater has a quench pressure of up to 12 bar and a maximum temperature of up to 1315°C (2400°F). The fully automatic furnace has a load size of 24 inches wide x 36 inches deep x 24 inches high with a load weight of 680 kilograms (1,500 lb).
Ipsen International (www.ipsen-intl.com) is a key manufacturer of vacuum and atmosphere heat-treating furnaces for the thermal processing market.