Dylon Industries Inc.
Dyforge 880 is a heavy-duty ultra-high temperature forging lubricant. It is water-based and contains micro-fine graphite and a special proprietary binder additive package. It is designed to forge difficult, warm or hot ferrous, super alloy and powder metal parts with exceptional abilities on aerospace forgings, precision forgings, and net forgings. It can be used on dies with temperatures from 150-1300°F (66-704°C). The lubricant's enhanced properties provide an extension in die life that results in less downtime, reduced scrap rates, and improved cycle times and increased pieces manufactured per hour.www.dylon.com