Euclid Heat Treating (Cleveland, Ohio) has installed an automated nitriding system from Super Systems Inc. (Cincinnati, Ohio).
Euclid Heat Treating(Cleveland, Ohio) has installed an automated nitriding system from
Super Systems Inc.(Cincinnati, Ohio). The nitriding system, which includes a combination of SSi controls, gas analyzers and software, provides a fully automated lights-out process.
The control system provides automatic cycle controls with less operator involvement, creating an error-free environment and delivering more repeatable and traceable products.