Ipsen recently shipped an H3636 2-bar TurboTreater® furnace
to a commercial heat-treatment company located in the southeastern U.S. The high-temperature
furnace included a 2-inch-thick carbon-composite/graphite-felt hot zone with a
nominal work zone of 24 inches x 24 inches x 36 inches and a gross load
capacity of 1,500 pounds, configured for 460 volts, 60 hertz, three phase. The
furnace was equipped with the user-friendly CompuVac® supervisory control
system as well as a nitrogen and argon partial-pressure system.