Penn Stainless Products

High-Temperature Alloy

330 Plate and Processed Flat Bar is ideally suited for demanding, high-temperature, high-pressure applications such as thermal processing, ore processing and power generation. Alloy 330 provides superior resistance to corrosion and heat exposure in high-temperature environments up to 2200°F and is extensively used where resistance to the combined effects of thermal cycling and carburization is necessary. It is available in thickness from 3/16 to ¾ inches and can be custom fabricated to any shape or size. Alloy 330 is an austenitic, nickel-chromium-iron-silicon alloy with excellent corrosion resistance. It also has a low coefficient of expansion, excellent ductility and high strength.

Did you enjoy this article? Click here to subscribe to Industrial Heating Magazine 

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

What does it take to make a bearing?

Here is an image gallery depicting the steel bearing production cycle, following a range of 10 steps from material selection to post-process verification.

Podcasts

In this month's podcast, Dan Herring and IH Editor Reed Miller discuss cast aluminum..


Sponsored By: 

More Podcasts

THE MAGAZINE

Industrial Heating

May Cover

May 2013

Take a look at the newest issue of Industrial Heating Magazine!
Table Of Contents Subscribe

Poll Question

What Industrial Heating website features do you utilize the most?
Poll Archive

THE INDUSTRIAL HEATING STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\IH\vacuum-heat-treatment.gif
Vacuum Heat Treatment

Vacuum Heat Treatment is a comprehensive introduction and technical resource for vacuum processes and equipment, focusing on subjects that engineers, heat treaters, quality assurance personnel and metallurgists need to know.

More Products

Clear Seas Research

CS-OflRGB1.gifWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Employment Marketplace

Employment Marketplace

STAY CONNECTED

Facebook IconTwitter IconYoutube IconLinkedin Icon