Demanding specifications often require 100% testing together with checking the homogeneity of workpieces. For measurements of hardness, it is either not cost effective or not possible at all to perform both with traditional testing methods. The solution can be portable hardness testers but often only if reliable conversions into conventional hardness scales are available or can be created.
WANT TO READ MORE?
SIGN UP TODAY...IT'S FREE!
(and takes less than a minute)


More


With access to over one million professionals and more than 60 industry-specific publications,