- BLOG
Alcoa announced that its Alcoa Power and Propulsion business has been awarded a 10-year, $360 million contract by Lockheed Martin to supply advanced patented 7805 alloy aluminum die forgings for the F-35 Joint Strike Fighter (JSF) program.