Electromagnetic Testing Validates Heat-Treated Part Condition

January 11, 2004
/ Print / Reprints /
ShareMore
/ Text Size+
Electromagnetic testing provides a qualitative test having the capability to accurately sort parts based on hardness, case depth, alloy and part shape.
WANT TO READ MORE?
(and takes less than a minute)

Multimedia

Videos

Image Galleries

2013 Product Roundup

The Product Roundup is a showcase of some of the best products and technologies the thermal-processing industry has to offer.  Industrial Heating has rounded up these advanced, energy-efficient and cost-effective items in one special section  for easy reference.

Podcasts

The Heat Treat Doctor, Dan Herring, and IH Editor Reed Miller get together each month to talk technical. August’s podcast features a discussion about backfill and partial-pressure gases. Sponsored by: 

More Podcasts

Industrial Heating

Cover Image

2014 August

August's issue of Industrial Heating includes a special feature on the latest aluminum scrap recycling plant technology, as well as a look at some of the latest heat treatment products and innovations.

Table Of Contents Subscribe

Social Media

What social-media site do you use most frequently?
View Results Poll Archive

THE INDUSTRIAL HEATING STORE

EDM_cover.gif
Everyday Metallurgy

If you have ever wished there was something people could read to help them better understand what you do, this is the book for you.

More Products

Clear Seas Research

CS-OflRGB1.gifWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Employment Marketplace

Employment Marketplace

STAY CONNECTED

Updated FacebookTwitter imageYoutube IconLinkedin Icon