This five-minute video provides a technical explanation of the benefits of the IntensiQuench (IQ) process. These benefits include surface compressive stresses and the minimization of part distortion while increasing surface hardness up to 10%, core hardness 20-50%, strength by 30% and toughness as much as 300%.